In the _Pattinson_ process the argentiferous lead is melted down in the central cast iron kettle of a series 8-15, placed one next to the other, each having a capacity of 9-15 tons and a separate fire-place. The crystals of impoverished lead which fall to the bottom, upon coaling the charge, are taken out with a skimmer and discharged into the neighbouring kettle (say to the right) until about two-thirds of the original charge has been removed; then the liquid enriched lead is ladled into the kettle on the opposite side. To the kettle, two-thirds full of crystals of lead, is now added lead of the same tenor in silver, the whole is liquefied, and the cooling, crystallizing, skimming and ladling are repeated. The same is done with the kettle one-third filled with liquid lead, and so on until the first kettle contains market lead, the last cupelling lead. The intervening kettles contain leads with silver contents ranging from above market to below cupelling lead. The original Pattinson process has been in many cases replaced by the Luce-Rozan process (1870), which does away with arduous labour and attains a more satisfactory crystallization. The plant consists of two tilting oval metal pans (capacity 7 tons), one cylindrical crystallizing pot (capacity 22 tons), with two discharging spouts and one steam inlet opening, two lead moulds (capacity 3½ tons), and a steam crane. Pans and pot are heated from separate fire-places. Supposing the pot to be filled with melted lead to be treated, the fire is withdrawn beneath and steam introduced. This cools and stirs the lead when crystals begin to form. As soon as two-thirds of the lead has separated in the form of crystals, the steam is shut off and the liquid lead drained off through the two spouts into the moulds. The fire underneath the pot is again started, the crystals are liquefied, and one of the two pans, filled with melted lead, is tilted by means of the crane and its contents poured into the pot. In the meantime the lead in the moulds, which has solidified, is removed with the crane and stacked to one side, until its turn comes to be raised and charged into one of the pans. The crystallization proper lasts one hour, the working of a charge four hours, six charges being run in twenty-four hours.